Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50% RH; ISO 527-1 |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Radici Radilon® S 38M (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Radici Radilon® S LHS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | |
Ineos ABS NOVODUR® KU 2-5296 ABS, Extrusion Grade
(discontinued **) Extrusion grade, flame retardant, medium toughness, suitable for thermoforming. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Extruded sheets and profiles.Information provid.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
Gichem GILAC C120/T Acrylonitrile Butadiene Styrene
(discontinued **) ABS with excellent thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | (50mm/min); ISO 527-2/1A |
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 2 in/min; ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-30 Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D-638 |
Axiall 3121 Rigid PVC, Extrusion Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui.. |
|||
Tensile Strength, Yield | 45.0 - 60.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
6530 - 8700 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50mm/min; ISO 527 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min |
Polimeri Europa SINKRAL D160 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-08-09-25 Very high heat injection moulding grade with good flow. Permits production of complex, thin walled.. |
|||
Tensile Strength, Yield | 45.0 - 86.0 MPa | 6530 - 12500 psi | Average value: 73.7 MPa Grade Count:5 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 45.0 MPa | 6530 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |