Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.03 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 9.03 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 9.02 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6819 PC (Asia Pacific) Medium flow, UV stabilised, high impact grade of polycarbonate.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® VR2820 PC (Europe-Africa-Middle East) VR 2820 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. |
|||
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 9.03 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 9.03 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Izod Impact, Notched | 9.00 J/cm @Thickness 3.17 mm |
16.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 9.00 J/cm @Thickness 3.20 mm |
16.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC0700 PC PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC0703 PC PC0703 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC0703 PC (Asia Pacific) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC0800 PC (Asia Pacific) PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC0800 PC (Europe-Africa-Middle East) PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ISO 180/4A |
Styron CALIBREâ„¢ 302V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are availab.. |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB890 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | ASTM D256 |
Aclo Accucomp Polycarbonate POL051L Medium Viscosity |
|||
Izod Impact, Notched | 9.00 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ715 Polycarbonate, UV Stabilized UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |