Material Notes:
Information provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 0.910 - 0.930 g/cc
0.0329 - 0.0336 lb/in³
ISO 1183
Melt Flow 1.0 - 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 - 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D >= 45
>= 45
ASTM D 2240
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D 638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D 638
Elongation at Break 500 %
500 %
ASTM D 638
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ISO 306
Brittleness Temperature -70.0 °C
-94.0 °F
ASTM D 746
Processing Properties Metric English Comments
Melt Temperature >= 115 °C
>= 239 °F
Users viewing this material also viewed the following: