Polymer Property : Melt Temperature = 239 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature >= 115 °C
>= 239 °F
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound
Information provided by PolyPlastic Group.
Melt Temperature 115 - 125 °C
239 - 257 °F
Borealis LE0511 Polyethylene Compound, Crosslinkable, Semiconductive
LE0511 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0511 is intended for strippable outer semi conductive s..
Melt Temperature 115 - 125 °C
239 - 257 °F
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound
Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet..
Melt Temperature 115 °C
239 °F
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid..
Melt Temperature 115 - 125 °C
239 - 257 °F
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound
Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry..
Melt Temperature 115 - 120 °C
239 - 248 °F
BecauseWeCare BF90 Biodegradable Plastic
Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari..
Melt Temperature 115 - 290 °C
239 - 554 °F
Average value: 191 °C Grade Count:12
Overview of materials for Ethylene Butyl Acrylate