Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO 294-4
Melt Flow 0.50 - 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 - 1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
ISO 5272
Elongation at Break 7.4 %
7.4 %
ISO 527
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Charpy Impact Unnotched 5.50 J/cm²

@Temperature -40.0 °C
26.2 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
7.00 J/cm²

@Temperature 20.0 °C
33.3 ft-lb/in²

@Temperature 68.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²

@Temperature -40.0 °C
4.28 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
2.10 J/cm²

@Temperature 20.0 °C
9.99 ft-lb/in²

@Temperature 68.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C
14.4 µin/in-°F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 148 °C
298 °F