Polymer Property : Melt Temperature = 298 °F
Polymer Property :
Melt Temperature =
298 °F
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Melt Temperature
148
°C
298
°F
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
Information provided by PolyPlastic Group.