Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYfill PPC GF15030 PD1 VT2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polykemi AB
Trade Name POLYfill
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYfill PPC GF15030 PD1 VT2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Filler Content 30 %
30 %
±2%; Polykemi
Melt Index of Compound 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 70.0 MPa
<= 10200 psi
ISO/R527
Elongation at Break 4.0 %
4.0 %
ISO/R527
Flexural Strength <= 110 MPa
<= 16000 psi
ISO 178
Flexural Modulus 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
120°C/h; ISO 75/1
Vicat Softening Point 120 °C

@Load 5.001 kg
248 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1