Material Notes:
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm

@Thickness 3.175 mm
0.0010 - 0.0020 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
16900 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 7.853 GPa
1139 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ASTM D648