| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Maxxam™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
| Melt Flow | 7.3 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
7.3 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
Procedure A; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 53.1 MPa | 7700 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 10 % | 10 % | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
| Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
| Izod Impact, Notched | 1.50 J/cm <br>@Thickness 3.18 mm,<br> Temperature 23.0 °C |
2.81 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Gardner Impact | 12.4 J <br>@Thickness 3.18 mm,<br> Temperature -23.0 °C |
9.15 ft-lb <br>@Thickness 0.125 in,<br> Temperature -9.40 °F |
ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 157 °C <br>@Thickness 3.18 mm |
315 °F <br>@Thickness 0.125 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Impact Modifier | |
| Appearance | Natural Color | |
| Features | Chemically Coupled | |
| Impact Modified | ||
| Filler / Reinforcement | Glass Fiber Reinforcement | |
| Unspecified FillerReinfor., 20% Filler by Weight | ||
| Forms | Pellets | |
| Generic Material | PP, Unspecified | |
| Generic Name | Polypropylene, Unspecified (PP, Unspecified) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |