Material Notes:
FormulationNordel® IP 4725P
Physical Properties Metric English Comments
Density 1.283 g/cc
0.04635 lb/in³
Mooney Viscosity 44

@Temperature 100 °C
44

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Vulcanizate, Press cured, TC95 +3min at 160°C
Hardness, Shore D 46
46
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 15.13 MPa
2194 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 213 %
213 %
Vulcanizate, Press cured, TC95 +3min at 160°C
50% Modulus 0.00570 GPa
0.827 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00843 GPa
1.22 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.01448 GPa
2.100 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 53 %

@Temperature 100 °C
53 %

@Temperature 212 °F
Pellets cured MDR TC95 + 15 min at 160°C, 22 hr at 100°C; Method B