Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers PC-1035

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers PC-1035.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Injection Molding Grade Low Gloss PolycarbonateInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 23 g/10 min

@Load 3.80 kg,
Temperature 230 °C
23 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.7 MPa
10400 psi
chs 2 in/min; ASTM D638
Flexural Strength 105.8 MPa
15350 psi
Stress at 5% Strain, Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Flexural Modulus 2.76 GPa
401 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched NB
NB
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 108 °C
226 °F
0.125 in bar; ASTM D648
Vicat Softening Point 135 °C
275 °F
0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94 V-2
V-2
0.062 in and 0.125 in All Colors
Users viewing this material also viewed the following: