Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 12.4 J @Thickness 3.18 mm, Temperature -23.0 °C |
9.15 ft-lb @Thickness 0.125 in, Temperature -9.40 °F |
ASTM D3029 |
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Gardner Impact | 12.4 J @Thickness 3.18 mm, Temperature -23.0 °C |
9.15 ft-lb @Thickness 0.125 in, Temperature -9.40 °F |
ASTM D3029 |
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Gardner Impact | 12.4 J | 9.15 ft-lb | ASTM D5420-93 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J @Temperature -30.0 °C |
9.15 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Gardner Impact | 12.4 J | 9.15 ft-lb | ASTM D3029 |
Buckeye Polymers BP RPP 4516 C Polypropylene, 45% Mineral Filled Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag.. |
|||
Gardner Impact | 12.4 - 19.0 J | 9.15 - 14.0 ft-lb | Average value: 15.8 J Grade Count:4 |
Overview of materials for Polypropylene w/ 50% Calcium Carbonate This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and .. |