Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 12.4 J

@Thickness 3.18 mm,
Temperature -23.0 °C
9.15 ft-lb

@Thickness 0.125 in,
Temperature -9.40 °F
ASTM D3029
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Gardner Impact 12.4 J

@Thickness 3.18 mm,
Temperature -23.0 °C
9.15 ft-lb

@Thickness 0.125 in,
Temperature -9.40 °F
ASTM D3029
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Gardner Impact 12.4 J
9.15 ft-lb
ASTM D5420-93
Multibase Multi-ABS 801 Natural Extrusion Grade
Data provided by Multibase.
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J

@Temperature -30.0 °C
9.15 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Gardner Impact 12.4 J
9.15 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 4516 C Polypropylene, 45% Mineral Filled
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag..
Gardner Impact 12.4 - 19.0 J
9.15 - 14.0 ft-lb
Average value: 15.8 J Grade Count:4
Overview of materials for Polypropylene w/ 50% Calcium Carbonate
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and ..