Plastcom SLOVASTYR® B BT BK PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTYR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTYR® B BT BK PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy of shrinkage enables injection molding of round, cylindric or other hole products. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
STN EN ISO 1183-1
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
STN EN ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
STN EN ISO 527-2
Flexural Strength 85.0 MPa
12300 psi
STN EN ISO 178
Flexural Modulus 2.00 GPa
290 ksi
STN EN ISO 178
Charpy Impact Unnotched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 200 - 220 °C
392 - 428 °F
STN EN 11357-1
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 3344
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi
Descriptive Properties Value Comments
Color Black