Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B BT Polyethylene Terephthalate FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | STN EN 11357-1 |
Plastcom SLOVASTYR® B BT BK PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Melting Point | 210 - 220 °C | 410 - 428 °F | ISO 11357-1 |
Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Appl.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 215 - 220 °C | 419 - 428 °F | Average value: 217 °C Grade Count:7 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | Average value: 219 °C Grade Count:6 |
Overview of materials for Nylon, Barrier Film Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | crystalline melting point; Hot Stage Microscope |
Honeywell Capran® 518 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig.. |
|||
Melting Point | 217 - 220 °C | 423 - 428 °F | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | Average value: 220 °C Grade Count:24 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |