Techmer ES Plastiblend® ABS LG UV

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS LG UV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 36.5 MPa
5300 psi
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
Flexural Yield Strength 71.7 MPa
10400 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature 72.8 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature 163 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C
169 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB