Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP)
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Izod Impact, Notched 0.427 J/cm

@Temperature 23.0 °C
0.800 ft-lb/in

@Temperature 73.4 °F
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
unannealed; ASTM D648
Descriptive Properties Value Comments
Process Film
Thermoforming