Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D 790 |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790A |
BP Amoco Acctuf® 3950 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Low gloss, High melt flow, Low temp impact, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fro.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.31 - 10.3 GPa | 190 - 1500 ksi | Average value: 4.09 GPa Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790B |
Ineos R35C-01 Polypropylene Random Copolymer Grade R35C-01 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PP1-2002ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All in.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790B |
Ineos L34N-00 Polypropylene Impact Copolymer Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Flexural Modulus | >= 1.31 GPa | >= 190 ksi | ASTM D790 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 50 mm/min span, 5 mm/min, 1 % secant; ASTM D790 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 50 mm/min span, 5 mm/min, 1 % secant; ASTM D790 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 50 mm/min span, 5 mm/min, 1 % secant; ASTM D790 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Flexural Modulus | 1.31 - 1.455 GPa | 190 - 211.0 ksi | UV Postcure; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |
|||
Flexural Modulus | 1.31 - 1.59 GPa | 190 - 230 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790A |
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |