Material Notes:
Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipping containers (closed head and/or open head) ranging in sizes from 10 to 114 litres (2.5 to 30 gallons). It is also used in other large parts such as toys (sleds), gasoline tanks for lawn mowers or snow blowers, etc.Petromont HDPE 1201 is a medium molecular weight hexene modified resin with a broad molecular weight distribution offering an excellent combination of stress cracking resistance, toughness, mouldability, parison stability and rigidity as well as excellent resistance to most chemicals.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 600 hour
>= 600 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.12 g/10 min
0.12 g/10 min
I<sub>2</sub>; ASTM D1238
13 g/10 min
13 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.8 MPa
3600 psi
ASTM D638
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
ASTM D790
Izod Impact, Notched >= 1.07 J/cm
>= 2.00 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Blow Molding