Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.12 g/10 min | 0.12 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 1201 High Density Polyethylene Resin Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipp.. |
|||
Melt Flow | 0.12 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.12 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing net, wire & cable insulators, auto parts, pipesMeets FDA requirements as listed.. |
|||
Melt Flow | 0.12 - 0.18 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.12 - 0.18 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC PH162 HDPE Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f.. |
|||
Melt Flow | 0.12 g/10 min | 0.12 g/10 min | Condition E; ASTM D 1238 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 0.12 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p.. |