Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPC-20T Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer) Information provided by PolyOne |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 20-2501 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 20-3401 Description: Random Copolymer Polypropylene, ClarifiedInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 20-3401 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Type IV bar at chs 2 in per min; ASTM D638 |
Network Polymers NPP 50-2053 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Spartech Marballoy Marbleized Thermoplastic Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Spartech Ultros SRP Co-Extruded Skid-Resistant PE Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 6510E Injection Molding Polypropylene Impact CopolymerApplications: General purpose injection molding of consumer products, household appliances, lawn and garden items and medical components.Formolene 6510E is a higher impact, medium st.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Total PSI 940E Impact Polystyrene Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Benzoflex T-150 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Compression molded parts prepared according to ASTM D 1928 Procedure C.; ASTM D638 |
Dow CONTINUUM™ DGDC-2480 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® 3272 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This high flow resin allows fast injection cycles and provides good impact strength, rigidity, and warpage resistance. This product me.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3590 psi | ASTM D412 |
ACC EP AEP EPI Engineered Polymers EP AEP is a new generation of Internetwork Polymers of polyurea and Epoxy, “Powered by Reactamine® Technology”. EP AEP was developed for a colorfast floor for both residential and industrial appl.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Total PPC 4280W Polypropylene, Impact Copolymer ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hard.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B901 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 24.8 MPa | 3600 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |