Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Petromont 1201 High Density Polyethylene Resin Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipp.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Tangent; ASTM D790 |
Flint Hills 23T2A Random Copolymer Polypropylene Features: Clarified, autoclave and good impact strength. Product does not contain animal derived components.Applications: Designed for Blow molding and ThermoformingInformation provided by Flint H.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Tangent; ASTM D790 |
Flint Hills AP6120-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Hyosung Topilene J340 PP J340 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Hyosung Topilene R701 PP R701 Injection Random CopolymerApplications:High transparent productISBM bottleCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Hyosung Topilene R701 PP R701 Random CopolymerApplications: General injectionCharacteristics: TransparenceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Hyosung Topilene R701G PP R701G Random CopolymerApplications:Disposable syringeGamma-ray sterilizationCharacteristics:Gamma-ray resistancyHigh transparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
Hyosung Topilene R801H PP R801H Injection Random CopolymerApplications:High transparent productLarge articlesCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Tangent; ASTM D790 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Test 1 |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | 15mm/min; ASTM D790 |
LG Chemical LUTENE-H BE0350 HDPE Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790A |
Ineos L10G-00 Polypropylene Impact Copolymer L10G-00 is a barefoot polypropylene impact copolymer designed for injection molding applications. It offers excellent impact resistance, high flexural modulus and good processability. This material .. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | |
Zylog Hipolyene® 7635 MI Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Rilsan® PA 11 BESNO MED Nylon 11 Rilsan® PA 11 BESNO MED is a polyamide produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specially designed to meet the stringent requirements.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | Test 1 |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Flexural Modulus | 1.13 GPa | 164 ksi | ASTM D790 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |