Material Notes:
PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistance. The gel-like viscosity and good depth of cure make it ideal for use on vertical surfaces or where large gaps are involved. Features & Benefits: Cure on demand Non-drip Flexible, good impact resistance Fast curing with low-power lamps 100% solids, no solvents Excellent adhesion to metal and glass Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
uncured
Viscosity 185000 cP

@Temperature 25.0 °C
185000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength 16.5 MPa
2390 psi
ASTM D2095
Elongation at Break 60 %
60 %
Adhesive Bond Strength 10.0 - 11.0 MPa
1450 - 1600 psi
Glass/steel, Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Optical Properties Metric English Comments
Refractive Index 1.47
1.47
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.0

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Strength 12.0 kV/mm
305 kV/in
Processing Properties Metric English Comments
Cure Time 0.0833 min
0.00139 hour
fixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless Gel
Uncured
Cure Wavelength (nm) 365-400
Maximum Gap Fill (mm) 2.5
Strength Retention 10% at 200°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
95% at 50°C
Relative to 0°C