Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 185000 cP @Temperature 25.0 °C |
185000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |