Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 121 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Intermittent use; ASTM D746-98
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
Maximum Service Temperature, Air 121 °C
250 °F
Continuous
Pyrotek TS-114 Thermoset Electrical Insulation Product (Nema Grade: GPO-3)
Glass reinforcement, Polyester resin, Red color. Flame retardant. Excellent arc and track resistance. UL recognized.Information provided by Pyrotek.
Maximum Service Temperature, Air 121 °C
250 °F
Resinlab® CYNERGY CA6405 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Maximum Service Temperature, Air 121 °C
250 °F
Continuous
Dielectric Polymers NT-101PLE Double Liner Tape  (discontinued **)
Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner.Features: Polyethylene interliner permits selective diecuttingPlasticizer migration resistantChemica..
Maximum Service Temperature, Air 121 °C
250 °F
Cured
Resinlab® AR 4315 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
Maximum Service Temperature, Air 121 °C
250 °F
Cured
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version..
Maximum Service Temperature, Air 121 °C
250 °F
dry
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black
Information provided by ITW Devcon
Maximum Service Temperature, Air 121 °C
250 °F
wet
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber
Information provided by ITW Devcon
Maximum Service Temperature, Air 121 °C
250 °F
Henkel Hysol PL 696 Film Adhesive
Epoxy-based structural film adhesive designed primarily for out-of-autoclave curing process applications requiring low cure temperatures as well as low curing pressures and is also available in ligh..
Maximum Service Temperature, Air 121 °C
250 °F
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System
Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures..
Maximum Service Temperature, Air 121 °C
250 °F
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound
Master Bond Polymer System EP21TDC-2 is a two component highly flexible epoxy resin compound for high performance bonding, sealing, coating and encapsulation. It is formulated to cure fully at ambie..
Maximum Service Temperature, Air 121 °C
250 °F
Master Bond EP27 Low Temperature Curing Two Component Epoxy
Master Bond Polymer System EP27 is a unique two component epoxy formulation offers relatively fast cures at temperatures as low as 40°F and below, with curing times much shorter than currently exis..
Maximum Service Temperature, Air 121 °C
250 °F
See Note 2.
ChevronTexaco Multifak® AFB NLGI Grade 2
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Maximum Service Temperature, Air 121 °C
250 °F
Operating Temperature
Devcon Backing Compound Epoxy
Abrasion-Resistant SystemData provided by Ellsworth Adhesives.
Maximum Service Temperature, Air 121 °C
250 °F
ExxonMobil 375 NC Mobiltac
Mobiltac 375 NC, 325 NC and 275 NC extra high performance non-leaded, diluent-type, heavy-bodied open gear lubricants designed for a wide variety of open gear and mining applications. They contain a..
Maximum Service Temperature, Air 121 °C
250 °F
May be used to contain foods during baking above this temperature.
DuPont Teijin Films Mylar® HS Polyester Film, 80 Gauge (20 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe..
Maximum Service Temperature, Air 121 °C
250 °F
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a ..
Maximum Service Temperature, Air 121 °C
250 °F
for 30 mins
3M 2308 Performance Masking Tape
Scotch® Performance Masking Tape 2308 is general purpose masking tape for holding, bundling, sealing, general paint masking and a vast number of other jobs where a pressure-sensitive tape is needed..
Maximum Service Temperature, Air 121 °C
250 °F
Service
3M 7830 Thermal Transfer Polyester Label Material
3M™ Thermal Transfer Polyester Label Materials are thin profile, gloss polyester label stocks that offer excellent durability and moisture resistance. These label materials utilize 3M™ Adhesive 40..
Maximum Service Temperature, Air 121 °C
250 °F
cured 14 days @ 50% RH
3M AC-350 Class A-1 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Maximum Service Temperature, Air 121 °C
250 °F
cured 14 days @ 50% RH
3M AC-730 Class C-4 (168) Aerospace Sealant
3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a..
Maximum Service Temperature, Air 121 °C
250 °F
3M Scotch-Weld™ DP620NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesive DP-620NS is a back, long working time, two-component polyurethane. Formulated as 1:1 ratio liquids. With the squeeze of the trigger, or with automated dispensing..
Maximum Service Temperature, Air 121 °C
250 °F
for 30 mins
3M Scotch® 232 High Performance Masking Tape
Scotch® High Performance Masking Tape 232 is designed to be used in medium temperature paint bake operations.Information provided by 3M
Maximum Service Temperature, Air 121 °C
250 °F
3M Scotch-Weld™ DP-5106 Control Joint Sealant
3M™ Scotch-Weld™ Control Joint Sealant DP-5106 is a self-leveling, gray, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in duo-pak cartridges. With the squeeze of t..
Maximum Service Temperature, Air 121 °C
250 °F
Not cleared by FDA for food temperatures above this temperature.
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Maximum Service Temperature, Air 121 °C
250 °F
Henkel Hysol EA 9628 Film Adhesive
First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2
Maximum Service Temperature, Air 121 °C
250 °F
Intermittent
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Maximum Service Temperature, Air 121 °C
250 °F
Loctite® Durabond® M-11FL Urethane Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Maximum Service Temperature, Air 121 °C
250 °F
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive
Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig..
Maximum Service Temperature, Air 121 °C
250 °F
Master Bond UV15X-2 One Component, Non-Yellowing UV Curable Adhesive
Master Bond UV15X-2 is a one component, non-yellowing UV curable polymer system for high performance coatings, adhesives and sealants with exceptionally fast response to UV radiation. The cured coa..
Copyright © lookpolymers.com All Rights Reserved