Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 16.5 MPa | 2390 psi | ASTM D2095 |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | Optimum; FF; ASTM D638 |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | Dry Heat Aging 392°F; 336 hr; ASTM D865 |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 300; ISO 37 |
BASF Elastollan 1085 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 20; ISO 37 |
BASF Elastollan 1154 D KFFC TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |