Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CleanerA Surface Cleaner Permabond Cleaner A is a general purpose industrial cleaner for cleaning and degreasing surfaces prior to bonding with any Permabond adhesive. Where surfaces are greasy or dirty, wiping with CLEANER.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CSA Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It also enables fillets of cu.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET505 Epoxy Resin PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH167 Anaerobic Retainer Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM118 Anaerobic Threadlocker Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM161 Anaerobic Retaining Compound Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV620 UV-curable Adhesive PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV649 UV-curable Adhesive PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F807 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F816 Black Polyetheretherketone (PEEK) Liquid Dispersion VICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. The VICOTE F815 and F816Blk grades have been specificall.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA4246 Toughened Acrylic Adhesive PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV630 UV-curable Adhesive PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
Silikony Polskie Polsil E1 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
Silikony Polskie Polsil E2 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | No freezing |
3M Dyneon™ PFA 6910GZ Fluoroplastic Dispersion 3M™ Dyneon™ PFA 6910GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magni.. |
|||
Storage Temperature | 5.00 - 27.0 °C | 41.0 - 80.6 °F | 3 months |
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed.. |
|||
Storage Temperature | 5.00 - 27.0 °C | 41.0 - 80.6 °F | 3 months |
ACC QSil 58 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 58 is a red, high temperature, self-leveling, two-component silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section C.. |
|||
Storage Temperature | 5.00 °C | 41.0 °F | |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |