Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond Anti-Seize Compound Lubricant Permabond Anti-Seize is a superior grade assembly compound and high pressure lubricant. This high quality aluminum, copper and graphite based antiseize formula has unique particle shapes suspended i.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CSA Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It also enables fillets of cu.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET536 Epoxy Resin PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM160 Anaerobic Retaining Compound Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH050P Pure Anaerobic Threadsealant PERMABOND® LH050 PURE anaerobic pipe sealant is single component paste that cures only when in contact with metal parts and oxygen is excluded. The sealant fills up the entire space between male an.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH150 Anaerobic Threadsealant Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LM012 Anaerobic Threadsealant Permabond® LM012 is an unfilled, medium viscosity anaerobic adhesive. Its major benefit as related to other pipe sealants is that it is an unfilled resin that is compatible with hydraulic fluids. I.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond POP Polyolefin Primer Permabond® Polyolefin Primer has been developed for surface treatment of polyolefins, PTFE and silicones prior to bonding with Permabond® Cyanoacrylate adhesives. Due to their low surface energy, .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV640 UV-curable Adhesive PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F804 Black Polyetheretherketone (PEEK) Liquid Dispersion EVICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. VICOTE F804Blk has been specifically formulated to provi.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F805 Polyetheretherketone (PEEK) Liquid Dispersion The VICOTE F805 natural, F806 natural and F807Blk grades have been specifically formulated to provide a tough, resilient, high wear resistant coating with varying levels of lubricants on ferrous and.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Storage Temperature | 10.0 - 25.0 °C | 50.0 - 77.0 °F | |
Akzo Nobel Trigonox® C Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of pol.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A025 Anaerobic Retainer Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F810 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |