Mechanical Properties Metric English Comments
Adhesive Bond Strength 10.0 - 11.0 MPa
1450 - 1600 psi
Glass/steel, Shear
Permabond UV625 UV-curable Adhesive
PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan..
Adhesive Bond Strength 9.00 - 11.0 MPa
1310 - 1600 psi
FRP Glass/Epoxy, Shear; ASTM D1002
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..