Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window

Category Ceramic , Glass , Optical , Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Sheet
Manufacturer Parker Chomerics Tecknit
Trade Name Teckshield®-F
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIELD-F windows have proven to be effective in TEMPEST qualified Visual Display Units, as well as in printers and enclosures requiring large viewing apertures. A special low-resistance mesh is laminated between two layers of glass or acrylic. The edge termination between the window mesh and the enclosure is designed to provide uniform mesh-to-enclosure continuity around the entire perimeter of the shielding aperture.Application Information: TECKSHIELD-F high-performance flat windows are designed for enclosures requiring superior shielding against EMI radiation or susceptibility. They provide maximum EMI protection and high optical clarity for teleprinters, digital, graphic, and other flat displays. TECKSHIELD-F windows can also be economically matched to most visual display units to minimize image distortion and to maximize shielding effectiveness.Information provided by Chomerics
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Acrylic
80.0 °C
176 °F
Glass
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass
-55.0 °C
-67.0 °F
Acrylic
Electrical Properties Metric English Comments
Shielding Effectiveness 40 dB

@Frequency 1.00e+10 Hz
40 dB

@Frequency 1.00e+10 Hz
Plane Wave
55 dB

@Frequency 100000 Hz
55 dB

@Frequency 100000 Hz
H-Field
60 dB

@Frequency 1.00e+9 Hz
60 dB

@Frequency 1.00e+9 Hz
Plane Wave
120 dB

@Frequency 1.00e+7 Hz
120 dB

@Frequency 1.00e+7 Hz
E-Field