Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shielding Effectiveness = 40 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 40 dB

@Frequency 10000 Hz
40 dB

@Frequency 10000 Hz
H-Field
P & P Technology Aluminum 5056 (AMS 4182) Knitted Cored Shielding Mesh
Product has a diameter of 0.11mm.Information provided by P & P Technology
Shielding Effectiveness 40 dB

@Frequency 10000 Hz
40 dB

@Frequency 10000 Hz
H-Field
P & P Technology Stainless Steel (Alloy 304) Knitted Cored Shielding Mesh
Product has a diameter of 0.11mm.Information provided by P & P Technology
Shielding Effectiveness 40 dB

@Frequency 1.00e+9 Hz
40 dB

@Frequency 1.00e+9 Hz
With 360° ground termination
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield
Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em..
Shielding Effectiveness >= 40 dB

@Frequency 1.00e+9 Hz
>= 40 dB

@Frequency 1.00e+9 Hz
Parker Chomerics METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Woven Wire ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Aluminum OnlyInformation provided by Chomerics
Shielding Effectiveness 40 dB

@Frequency 100000 Hz
40 dB

@Frequency 100000 Hz
H-Field
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.001" Diameter Wire, Allycarbonate EMI Shielding Window
Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig..
Shielding Effectiveness 40 dB

@Frequency 1.00e+10 Hz
40 dB

@Frequency 1.00e+10 Hz
Plane Wave
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.002" Diameter Wire, Allycarbonate EMI Shielding Window
Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig..
Shielding Effectiveness 40 dB

@Frequency 1.00e+10 Hz
40 dB

@Frequency 1.00e+10 Hz
Plane Wave
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window
Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE..
Shielding Effectiveness 40 dB

@Frequency 1.00e+9 Hz
40 dB

@Frequency 1.00e+9 Hz
1/8 thickness
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Shielding Effectiveness 40 - 45 dB

@Frequency 1.50e+10 - 1.80e+10 Hz
40 - 45 dB

@Frequency 1.50e+10 - 1.80e+10 Hz
Master Bond MB600G Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600G is an aqueous based, sodium silicate system with graphite filler. It is intended for use in applications where moderate shielding effectiveness is required and cost is a more sign..
Shielding Effectiveness 40 - 50 dB

@Frequency 7.00e+9 - 1.80e+10 Hz
40 - 50 dB

@Frequency 7.00e+9 - 1.80e+10 Hz
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co..
Shielding Effectiveness 40 - 55 dB

@Frequency 2.00e+9 - 7.00e+9 Hz
40 - 55 dB

@Frequency 2.00e+9 - 7.00e+9 Hz
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co..
Shielding Effectiveness 40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co..
Shielding Effectiveness 40 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
40 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
15% glass; ASTM D4935
Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber
Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS..
Shielding Effectiveness 40 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
40 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
3% CNS; ASTM D4935
Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes
Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based n..
Shielding Effectiveness 40 dB

@Frequency 1.00e+9 Hz
40 dB

@Frequency 1.00e+9 Hz
360° Ground Termination
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield
Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight ..