Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx93FRSD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica PVC Polyvinylchloride A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Fea.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Henkel Frekote 44-NC Mold Release Agent A non-CFC release agent designed to provide multiple releases with no contaminating transfer. Can be used for the release of thermoplastics, thermosetting resins, boron, aramid, graphite / carbon fi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 164 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Features: Flame Retardant; Low Temperature Flexibility; Moisture ResistantUses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW Processing Method: .. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 6500-85 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Maximum Service Temperature, Air | 60.0 - 80.0 °C | 140 - 176 °F | |
Sylvin Technologies 504 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | <= 60.0 °C | <= 140 °F | Laundering Resistance |
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Maximum Service Temperature, Air | 60.0 - 80.0 °C | 140 - 176 °F | long term; EMS |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | long term |
Ensinger PVC Polyvinylchloride (PVC) Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Colorite Polymers CS6041GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP012202 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP012603 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP021502 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP024408 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products FP024402 and FP024408 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra remova.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP083 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP531 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FS028 Clear Polystyrene Label Products 3M™ Clear Polystyrene Label Products are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, which is a high c.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV065 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV513 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FVS110S Static Cling Label Materials 3M™ Static Cling Label Materials are highly plasticized vinyl label materials available in white or clear that adhere to most clean smooth surfaces such as glass, painted metal, and most smooth pla.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FA031 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FS501 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FS502 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV02940N Textured Vinyl Label Products 3M™ Textured Vinyl Label Products are flexible and conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212 which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded .. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV0164R2 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M OFL010N Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JA508AF Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |