Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Pyrocast L-30 Moldable Refractory

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast L-30 Moldable Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommended for thicknesses up to 50 mm (2 in). If applied above 20°C, Pyrocast L-30 adheres well to metal and refractory surfaces.Applications Coatings Linings Refractory patching Sealing compound Collector bar sealsAdvantagesNon-wetting Good adhesion qualities Low shrinkage Low thermal conductivity Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.640 g/cc
0.0231 lb/in³
Solids Content 55 %
55 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.0800 W/m-K

@Temperature 204 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 399 °F
0.160 W/m-K

@Temperature 538 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.220 W/m-K

@Temperature 871 °C
1.53 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Maximum Service Temperature, Air 1093 °C
1999 °F
Shrinkage 2.00 %

@Temperature 1093 °C,
Time 86400 sec
2.00 %

@Temperature 1999 °F,
Time 24.0 hour
linear
6.00 %

@Temperature 1260 °C,
Time 86400 sec
6.00 %

@Temperature 2300 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Hot Gas Erosion Resistance Min 61 m/sec
Copyright © lookpolymers.com All Rights Reserved