Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV

Category Polymer , Adhesive
Manufacturer Parker Chomerics Tecknit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the resultant bond or seal of the material is flexible, resilient and conductive. Application Information: TECKNIT Conductive Adhesive-Sealants are recommended wherever an electrically conductive flexible bond and seal is required. The main consideration for selecting the correct adhesive should be based on the galvanic coupling of metallic (or conductive) materials. Excellent practices and recommendations can be obtained by reviewing MIL-STD- 1250. The Adhesive-Sealants are also used to join and install a variety of conductive elastomers and porous or open wire mesh gaskets.Information provided by Chomerics
Mechanical Properties Metric English Comments
Shear Strength >= 0.414 MPa
>= 60.0 psi
Cured; ASTM D1002
Peel Strength >= 0.526 kN/m
>= 3.00 pli
Silicone Aluminum; Cured; ASTM D1876
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Cured
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Cured
Shrinkage <= 31 %
<= 31 %
Cured
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Cured; QAP-1017
Processing Properties Metric English Comments
Cure Time 10100 min
168 hour
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
followed by 24 hr @ 100°C
Pot Life 4.0 min

@Temperature 25.0 °C
4.0 min

@Temperature 77.0 °F
Shelf Life 9.00 Month
9.00 Month
Unopened Container
Descriptive Properties Value Comments
Color Beige
Consistency Paste
Filler AG/Glass
Final Condition Flexible
Mix Ratio 49:1
Number of Components Two
Resin Silicone
Volume 13.6 in3
Weight 16 oz