Polymer Property : Peel Strength = 0.526 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.526 - 0.877 kN/m
3.00 - 5.00 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FA112 Destructible Acetate Label Products
3M™ Destructible Acetate Label Products FA102 and FA112 offer consistent, high quality film that fractures when attempting label removal from many surfaces. These acetate labels utilize 3M™ Adhesi..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FL015 Lexan Label Product
3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high ..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FM099 Indoor UL Recognized Matte Silver Polyester Label Product
3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FM127 Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FM16K Indoor UL Recognized Computer Imprintable White Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FP021 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FV092R Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FV094 Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
3M Scotchcal™ 3690 Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Glass
3M Scotchcal™ 50-27 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Glass
3M Scotchcal™ 50-745 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Polypropylene
3M Scotchcal™ ElectroCut™ 7125-13 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Polypropylene
3M Scotchcal™ ElectroCut™ 7125-15 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Polypropylene
3M Scotchcal™ ElectroCut™ 7125-57 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to FRP
3M Scotchlite™ 680-75 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to FRP
3M Scotchlite™ 680-81 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear..
Peel Strength 0.526 kN/m
3.00 pli
Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method
3M 7032 Screen Printable Polyester Performance Label Products
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u..
Peel Strength 0.526 kN/m
3.00 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.526 - 0.701 kN/m
3.00 - 4.00 pli
Adhesion to Acrylic enamel
3M Controltac™ FN180Cv3-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength >= 0.526 kN/m
>= 3.00 pli
Adhesion to Acrylic panels
3M Envision™ 3635-70 Diffuser Film
2-mil, white vinyl film; Pressure sensitive adhesive adheres to rigid substrates; Create custom lighting effects for backlit applications; Control brightness and light distribution within light dist..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FA023 Matte Clear Acetate Label Products
3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FM022R Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FM113 Indoor UL Recognized Brushed Silver Polyester Label Products
3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FP010609 Matte White Polypropylene Label Product
3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3..
Peel Strength 0.526 kN/m
3.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
3M FV033 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Glass
3M Scotchcal™ 50-78 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Glass
3M Scotchcal™ 50-82 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Polypropylene
3M Scotchcal™ ElectroCut™ 7725-46 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
Peel Strength 0.526 kN/m
3.00 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7980 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These..