Universal Wire Works Hastelloy W (AMS 5786) Filler Metal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Hastelloy W (AMS 5786) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hastelloy Alloy W welding wire is used extensively to join similar and dissimilar alloys of the cobalt and nickel base variety and other alloys used in high temperature service. Hastelloy Alloy W possesses good mechanical properties up to 1800°F and is used for welding turbine blades into rotor hubs and dissimilar alloys as mentioned above.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 5.0 %
5.0 %
Cobalt, Co <= 2.5 %
<= 2.5 %
Iron, Fe 6.0 %
6.0 %
Molybdenum, Mo 24 %
24 %
Nickel, Ni 63 %
63 %
Vanadium, V <= 0.60 %
<= 0.60 %