Material Notes:
Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended service life. This zero-pressure fluid provides precise, uniform temperature control to 550°F in closed-loop thermal oil systems where the heat transfer fluid is more than occasionally exposed to air. The crystal-clear OR fluid is comprised of a unique high-stability base plus high-performance oxidation inhibitor/stabilizer.Information provided by Paratherm Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.8863 g/cc
0.8863 g/cc
60/60; ASTM D1298
Density 0.866 g/cc

@Temperature 23.9 °C
0.0313 lb/in³

@Temperature 75.0 °F
ASTM D4052
Kinematic Viscosity at 40°C (104°F) 40.12 cSt
40.12 cSt
ASTM D445
Molecular Weight 360 g/mol
360 g/mol
average; ASTM D2502
Vapor Pressure 0.0654 bar

@Temperature 260 °C
49.0 torr

@Temperature 500 °F
Thermal Properties Metric English Comments
Heat of Vaporization 216.2 J/g
93.01 BTU/lb
calculated
CTE, linear 720 µm/m-°C

@Temperature 20.0 °C
400 µin/in-°F

@Temperature 68.0 °F
Boiling Point 333 °C
631 °F
atmospheric boiling point, 10% fraction; ASTM D1160
Maximum Service Temperature, Air 288 °C
550 °F
optimum use range
<= 316 °C
<= 600 °F
max. recommended film temperature
Minimum Service Temperature, Air 79.4 °C
175 °F
optimum use range
Pour Point -37.2 °C
-35.0 °F
ASTM D97
Flash Point 177 °C
350 °F
coc; ASTM D92
Electrical Properties Metric English Comments
Dielectric Strength >= 3.50 kV/mm
>= 88.9 kV/in
disk; ASTM D877
Dissipation Factor 0.00020

@Frequency 60 Hz
0.00020

@Frequency 60 Hz
ASTM D924
Descriptive Properties Value Comments
Appearance transparent, water-white
Autoignition 630°F
ASTM E659
Feedstock hydrotreated natural hydrocarbon
Fire point 395°F
ASTM D92, coc
Odor none
Total Acid Number 0.01
ASTM D664
Copyright © lookpolymers.com All Rights Reserved