Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.866 g/cc @Temperature 15.0 °C |
0.0313 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 10W-30 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Density | 0.866 g/cc @Temperature 15.0 °C |
0.0313 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 10W-30 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips 46 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 46 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear® 68 Refrigerant Oil Description: Conoco Hydroclear Refrigerant Oil is a high-quality ammonia refrigeration compressor lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Refrigerant Oil is spe.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear® 68 TCS Slideway lubricant Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant .. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips 46 Ultra-Clean Super Hydraulic Oil Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear® 350 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear® 68 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
BASF Pyrrolidine Pure Formula: C4H9NCAS: 123-75-1Description: Pyrrolidine pure is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: Tetrahydropyrrole, Perhydropyrrole, Azacyclopenta.. |
|||
Density | 0.866 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.866 g/cc @Temperature 15.0 °C |
0.0313 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Density | 0.866 g/cc @Temperature 15.0 °C |
0.0313 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Density | 0.866 g/cc @Temperature 23.9 °C |
0.0313 lb/in³ @Temperature 75.0 °F |
ASTM D4052 |
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic.. |