Material Notes:
Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports footwear and top-pieces. The features offered include:Durability Excellent surface definitionAbrasion resistanceFlex resistancePhthalate free TPU Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 37
Elongation at Break 350 %
350 %
ISO 37
100% Modulus 0.0220 GPa
3.19 ksi
ISO 37
300% Modulus 0.0340 GPa
4.93 ksi
ISO 37
Flexural Modulus 0.250 GPa
36.3 ksi
ISO 178
Tear Strength 220 kN/m
1260 pli
ISO 34B
Abrasion <= 35
<= 35
mm<sup>3</sup>; ISO 4649
Compression Set 25 %
25 %
ISO 815
Processing Properties Metric English Comments
Feed Temperature 25.0 - 35.0 °C
77.0 - 95.0 °F
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Middle Barrel Temperature 195 - 215 °C
383 - 419 °F
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Nozzle Temperature 195 - 210 °C
383 - 410 °F
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa
290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Screw Speed 20 - 80 rpm
20 - 80 rpm
Descriptive Properties Value Comments
Compression Ratio 2-3:1
L/D Ratio 20-25:1
Typical Screw Diameter 40-120 nm
Users viewing this material also viewed the following: