Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 3.50 kV/mm | 88.9 kV/in | ASTM D150 |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Dielectric Strength | 3.50 kV/mm | 88.9 kV/in | ASTM D150 |
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568.. |
|||
Dielectric Strength | 3.50 - 7.48 kV/mm | 88.9 - 190 kV/in | Average value: 4.71 kV/mm Grade Count:7 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Dielectric Strength | 3.50 kV/mm | 88.9 kV/in | ASTM D149 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Dielectric Strength | 3.50 kV/mm | 88.9 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 3.50 kV/mm @Thickness 3.00 mm |
88.9 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri.. |
|||
Dielectric Strength | 3.50 - 5.00 kV/mm @Temperature 90.0 °C |
88.9 - 127 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Dielectric Strength | >= 3.50 kV/mm | >= 88.9 kV/in | disk; ASTM D877 |
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic.. |