Polymer Property : Flash Point = 350 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 177 °C
350 °F
TOC
Palm Labs Adhesives Turbo Anti-Seize Aluminum Paste
TURBO ANTI-SEIZE – ALUMINUM is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot..
Flash Point 177 °C
350 °F
TOC
Palm Labs Adhesives Turbo Anti-Seize Copper Paste
TURBO ANTI-SEIZE – COPPER is a copper, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot..
Flash Point 177 °C
350 °F
TOC
Palm Labs Adhesives Turbo Anti-Seize Nickel Paste
TURBO ANTI-SEIZE – NICKEL is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where protec..
Flash Point 177 °C
350 °F
Lubriplate APG-75 Petroleum-Based Gear, Bearing, & Recirculating Oil
These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil..
Flash Point 177 °C
350 °F
Lubriplate MV-HO Petroleum-Based Heavy-Duty Hydraulic Oil
ISO 32 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Flash Point 177 °C
350 °F
coc; ASTM D92
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid
Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic..