Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 40.12 cSt
40.12 cSt
ASTM D445
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid
Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic..