Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 333 °C | 631 °F | atmospheric boiling point, 10% fraction; ASTM D1160 |
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic.. |