Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 350°F.HexWeb HRH-10 - NOMEX aramid paper reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 300°F.Features: Specifically designed for formability; Retains mechanical properties in the curved condition; Offers cost savings for curved panels.Applications: The HexWeb Nonmetallic Flex-Core cell confiation as opposed to the standard hexagonal cell honeycomb provides for exceptional formability into compound curvatures with reduced anticlastic curvature and controlled buckling of cell walls. When formed into tight radii, HexWeb Nonmetallic Flex-Core provides higher shear strengths than comparable hexagonal cores of equivalent density. HexWeb Nonmetallic Flex-Core applications exist wherever extreme curvature dictates a flexible cell geometry, e.g. radomes, ducts, leading edges of wings and stabilizers.
Physical Properties Metric English Comments
Density 0.0561 g/cc
0.00203 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 2.21 MPa
>= 320 psi
Bare, min
>= 2.28 MPa
>= 330 psi
Stabilized, min
2.83 MPa
410 psi
Bare, typ
2.96 MPa
430 psi
Stabilized, typ
Shear Modulus 0.0255 GPa
3.70 ksi
Plate Shear, W Direction, typ
0.0414 GPa
6.00 ksi
Plate Shear, L Direction, typ
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
0.827 MPa
120 psi
Plate Shear, W Direction, typ
>= 1.17 MPa
>= 170 psi
Plate Shear, L Direction, min
1.52 MPa
220 psi
Plate Shear, L Direction, typ
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Copyright © lookpolymers.com All Rights Reserved