Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 720 µm/m-°C @Temperature 20.0 °C |
400 µin/in-°F @Temperature 68.0 °F |
|
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic.. |