Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NextGen Adhesives G907-08 Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives G907-08 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC G907-08 is a low viscosity, electrically insulating, heat cured and 2-part adhesive systems designed for applications where temperature and chemical resistance is critical. The NGAC G907-08 is formulated with a color coded system to indicate unmixed, mixed and cured stages.Advantages and Applications: NGAC G907-08 provides strong and high impact bonds with a high level of chemical and temperature resistance. It bonds to a wide range of substrates including metals, glass and plastics. The NGAC G907-08 exhibits good wicking and provides excellent thermal shock resistance.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Viscosity 2000 cP
2000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Shear Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 110 °C
230 °F
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 125 °C
0.0833 hour

@Temperature 257 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Black
Mix Ratio by Weight (R/H) 100/10
Users viewing this material also viewed the following: