Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants 1251 Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants 500S (RT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants 716HT (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants 761G Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants NC-346 Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Recommended |
Nye Lubricants UniFlor 8132S (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
NextGen Adhesives P907-03 Fiber Optic Adhesive Description: NGAC P907-03 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
Tra-Con Tra-Bond F123LV Color Keyed High Temperature Epoxy Adhesive TRA-BOND F123LV is a fast cure, low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating s.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications .. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Dry |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Short Cycle |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Short Cycle |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Short Cycle |
DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Continuous |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Continuous |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Continuous |
Epoxy Technology EPO-TEK® B912-8 Epoxy Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Dry Service |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | |
Atom Adhesives AA-DUCT N02 Epoxy Adhesive AA-DUCT N02 is a single component, heat curing, conductive epoxy polymer that was designed for ease in handling. This high performance conductive polymer cures quickly at elevated temperatures makin.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® A3WG10 BK 00564 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade with high heat aging resistance for technical articles of very high stiffness.Information provided by BASF |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | Continuous service |
Dow Advanta® 3302 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |
|||
Maximum Service Temperature, Air | 175 °C | 347 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |