Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 50-0753

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-0753.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
chs 2 in/min; ASTM D638
Elongation at Break 950 %
950 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746