MV Labs MN300 MnCO3 Manganese(II) carbonate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs MN300 MnCO3 Manganese(II) carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 114.95 g/mol
114.95 g/mol
Descriptive Properties Value Comments
Assay 48% Mn
CAS Number 598-62-9
Form Pink powder
Purity 99.99+%
Typical Impurities Ca, Mg = 3 ppm