Material Notes:
DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Temperature 230 °C
5.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 25.2 MPa
3650 psi
2 in/min; ASTM D638
Elongation at Yield 40 %
40 %
at max load; ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm
20.0 ft-lb/in
ASTM D256
Gardner Impact 7.23 J
5.33 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
245 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D648
Users viewing this material also viewed the following: